Microstructure parameters of different activated carbon particles

SampleSBET (m2/g)SLangmuir (m2/g)St-plot (m2/g)DBET (nm)DBJH (nm)Vtotal (cm3/g)
2,006.13 2,657.60 1,782.17 1.9085 2.4067 0.957 
1,907.45 2,548.18 1,679.14 1.9184 2.3927 0.915 
1,199.65 1,563.17 1,068.61 1.8822 2.5685 0.565 
1,918.74 2,518.13 1,709.93 1.8737 2.4067 0.899 
1,278.53 1,698.70 1,154.11 1.8699 2.3889 0.598 
Zn 1,928.33 2,552.56 1,694.67 1.8969 2.3996 0.915 
SampleSBET (m2/g)SLangmuir (m2/g)St-plot (m2/g)DBET (nm)DBJH (nm)Vtotal (cm3/g)
2,006.13 2,657.60 1,782.17 1.9085 2.4067 0.957 
1,907.45 2,548.18 1,679.14 1.9184 2.3927 0.915 
1,199.65 1,563.17 1,068.61 1.8822 2.5685 0.565 
1,918.74 2,518.13 1,709.93 1.8737 2.4067 0.899 
1,278.53 1,698.70 1,154.11 1.8699 2.3889 0.598 
Zn 1,928.33 2,552.56 1,694.67 1.8969 2.3996 0.915 