Ferric hydroxide (FHO), which has high phosphate adsorption capacity, was prepared by precipitation at industrial scale and then fabricated via the drum granulation method with cross-linked poly(vinyl alcohol) as the binder. The optimum binder/FHO powder ratio was 0.6 for producing a granular adsorbent with a high phosphate adsorption capacity and stability. The Langmuir maximum adsorption capacities of powder and granular FHOs were 74.07 mg g−1 and 56.18 mg g−1 at pH 7.0 ± 0.2, respectively, which were higher than those of other reported phosphate adsorbents under neutral or acidic conditions. Phosphate-loaded granular FHO could be regenerated by NaOH solution. Columns containing the granular FHO were used for phosphate removal from ozonated secondary effluents of a municipal wastewater treatment plant at space velocity (SV) of 2 and 5 h−1. During more than 2 months’ operation, the average removal percentage of PO43– was more than 90% and the turbidity and concentration of CODMn in the effluents were lower than in the influents. In addition, energy dispersive X-ray results suggested that active sites inside the granular FHO were available for phosphate removal. The results demonstrated that granular FHO can be applied as an assist technology for phosphate removal from secondary effluents.

Supplementary data

You do not currently have access to this content.